Ni-Ir/Al2O3 负载型催化剂的制备及其用于水合肼分解制氢性能 |
| 杜宗罡, 徐涛, 李宁, 李文生, 邢钢, 巨璐, 赵利华, 吴华, 田育成 |
|
Preparation of Ni-Ir/Al2O3 Catalyst and Its Application for Hydrogen Generation from Hydrous Hydrazine |
| DU Zonggang, XU Tao, LI Ning, LI Wensheng, XING Gang, JU Lu, ZHAO Lihua, WU Hua, TIAN Yucheng |
| 图4 Al2O3载体和Ni60Ir40/Al2O3催化剂样品的N2吸/脱附等温线曲线 |
| Fig.4 N2 adsorption/desorption isotherm curves of Al2O3 carrier and Ni60Ir40/Al2O3 catalyst (STP—standard temperature and pressure, P is the partial pressure of nitrogen, and P0 is the saturated vapor pressure of nitrogen at liquid nitrogen temperature) |
|