露点对连续退火0.2%C-1.5%Si-2.5%Mn高强钢选择性氧化及脱碳的影响 |
| 金鑫焱, 储双杰, 彭俊, 胡广魁 |
|
Effect of Dew Point on Selective Oxidation and Decarburization of 0.2%C-1.5%Si-2.5%Mn High Strength Steel Sheet During Continuous Annealing |
| JIN Xinyan, CHU Shuangjie, PENG Jun, HU Guangkui |
| 图12 不同露点退火试样截面显微组织的OM像 |
| Fig.12 Cross-sectional OM images of the samples annealed at different dew points (a) -40oC (b) -20oC (c) 0oC (d) +10oC |
|