| 露点对连续退火0.2%C-1.5%Si-2.5%Mn高强钢选择性氧化及脱碳的影响 | 
| 金鑫焱, 储双杰, 彭俊, 胡广魁 | 
| Effect of Dew Point on Selective Oxidation and Decarburization of 0.2%C-1.5%Si-2.5%Mn High Strength Steel Sheet During Continuous Annealing | 
| JIN Xinyan, CHU Shuangjie, PENG Jun, HU Guangkui | 
| 图11 露点对钢板次表层C含量及脱碳层厚度的影响 | 
| Fig.11 Effects of dew point on C content (a) and decar-burization thickness (b) in the subsurface area (td1—thickness of total decarburization, td2—thickness of full decarburization) | 
|   |