露点对连续退火0.2%C-1.5%Si-2.5%Mn高强钢选择性氧化及脱碳的影响 |
| 金鑫焱, 储双杰, 彭俊, 胡广魁 |
|
Effect of Dew Point on Selective Oxidation and Decarburization of 0.2%C-1.5%Si-2.5%Mn High Strength Steel Sheet During Continuous Annealing |
| JIN Xinyan, CHU Shuangjie, PENG Jun, HU Guangkui |
| 图7 露点为-40℃退火试样TEM元素面分布结果 |
| Fig.7 EDS elemental mapping of the TEM sample annealed at dew point of -40oC |
|