| 露点对连续退火0.2%C-1.5%Si-2.5%Mn高强钢选择性氧化及脱碳的影响 | 
| 金鑫焱, 储双杰, 彭俊, 胡广魁 | 
| Effect of Dew Point on Selective Oxidation and Decarburization of 0.2%C-1.5%Si-2.5%Mn High Strength Steel Sheet During Continuous Annealing | 
| JIN Xinyan, CHU Shuangjie, PENG Jun, HU Guangkui | 
| 图3 不同露点退火试样Mn、Si元素深度分布 | 
| Fig.3 Mn (a) and Si (b) depth profiles of the samples annealed at different dew points | 
|   |