应变速率对X80管线钢铁素体/贝氏体应变分配行为的影响 |
| 王楠, 陈永楠, 赵秦阳, 武刚, 张震, 罗金恒 |
|
Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel |
| WANG Nan, CHEN Yongnan, ZHAO Qinyang, WU Gang, ZHANG Zhen, LUO Jinheng |
| 图11 不同应变速率下X80钢的应变硬化行为 |
| Fig.11 Strain hardening behaviors of X80 steel under different strain rates (a) true stress-strain curves (b) modified C-J model (εI-II is the strain at the transition point from stage I to stage II, and εII-III is the strain at the transition point from stage II to stage III) |
|