应变速率对X80管线钢铁素体/贝氏体应变分配行为的影响 |
| 王楠, 陈永楠, 赵秦阳, 武刚, 张震, 罗金恒 |
|
Effect of Strain Rate on the Strain Partitioning Behavior of Ferrite/Bainite in X80 Pipeline Steel |
| WANG Nan, CHEN Yongnan, ZHAO Qinyang, WU Gang, ZHANG Zhen, LUO Jinheng |
| 图1 基于X80管线钢金相组织建立代表性体积元(RVE)模型示意图及铁素体和贝氏体的真应力-应变曲线 |
| Fig.1 Schematics of making representative volume element (RVE) model (a-e) and true stress-strain curves of ferrite and bainite (f) (a) OM image (b) locally magnified OM image (c) binarization model (d) boundary line model (e) boundary condition of displacement (Ux and U represent the displacement of x-axis and boundary displacement direction, respectively) |
|