纳米多孔金属表面结构与成分的三维电子层析表征 |
| 段慧超, 王春阳, 叶恒强, 杜奎 |
|
Electron Tomography Analysis on the Structure and Chemical Composition of Nanoporous Metal Surfaces |
| DUAN Huichao, WANG Chunyang, YE Hengqiang, DU Kui |
| 图5 纳米多孔Au-Pt表面偏聚的3D分析 |
| Fig.5 3D analyses of surface segregation in nanoporrous Au-Pt (The thickness of the slices is 1 nm) (a) 3D reconstruction of the void in the surface (b) 3D reconstruction of Pt distribution around the void in Fig.5a (The color represents the intensity of the EDS signal of the Pt element, which gradually becomes more intense from blue to green) (c-f) multiple slices of 3D reconstructed chemical composition distribution on the surface of the void in Fig.5a (Crystallog-raphic planes with different indexes are determined and indicated) |
|