纳米多孔金属表面结构与成分的三维电子层析表征
段慧超, 王春阳, 叶恒强, 杜奎

Electron Tomography Analysis on the Structure and Chemical Composition of Nanoporous Metal Surfaces
DUAN Huichao, WANG Chunyang, YE Hengqiang, DU Kui
图2 低倍下纳米多孔Au结构和成分的三维(3D)重构结果
Fig.2 3D reconstructions of nanoporous gold structure (a) and chemical composition (b)