计算辅助高性能增材制造铝合金开发的研究现状与展望 |
| 高建宝, 李志诚, 刘佳, 张金良, 宋波, 张利军 |
|
Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review |
| GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun |
| 图5 Kou准则中裂纹敏感因子示意图[ |
| Fig.5 Schematic diagram of the crack susceptibility index (CSI) in the Kou criterion[ |
|