基于高通量制备的增材制造材料成分设计 |
| 张百成, 张文龙, 曲选辉 |
|
Composition Design of Additive Manufacturing Materials Based on High Throughput Preparation |
| ZHANG Baicheng, ZHANG Wenlong, QU Xuanhui |
| 图6 增材制造钢中主要组成元素和微观结构的变化[ |
| Fig.6 Changes of element composition (mass fraction, %) and microstructure of additive manufactured steel (a) ferritic stainless steel[ (c) maraging steel[ |
|