选区激光熔化NiTi形状记忆合金研究进展
|
|
杨超, 卢海洲, 马宏伟, 蔡潍锶
|
Research and Development in NiTi Shape Memory Alloys Fabricated by Selective Laser Melting
|
|
YANG Chao, LU Haizhou, MA Hongwei, CAI Weisi
|
|
图12 NiTi、不锈钢和人体组织的性能对比图;多孔结构的模型图以及SLM制备的多孔NiTi SMAs[37,38,63,90]
|
Fig.12 Comparisons of mechanical properties of NiTi SMAs, stainless steel, and human tissues (a), isometric view of the CAD model and image of SLM porous Ni45.2Ti54.8 (b)[38], CAD models with three different pore sizes and image of SLM porous Ni50.4Ti49.6 (c)[63], cellular lattice structure and image of SLM porous Ni50.6Ti49.4 (d)[90], and CAD models and image of the SLM Ni50.3Ti49.7 gyroid cellular structure (e) (U-GCS: uniform gyroid cellular structure, Y-GCS: graded gyroid structure with the density gradient along y-axis, Z-GCS: graded gyroid structure with density along gradient z-axis)[37]
|
|
|
|
|