选区激光熔化NiTi形状记忆合金研究进展
杨超, 卢海洲, 马宏伟, 蔡潍锶

Research and Development in NiTi Shape Memory Alloys Fabricated by Selective Laser Melting
YANG Chao, LU Haizhou, MA Hongwei, CAI Weisi
图7 热处理后SLM NiTi SMAs的TEM像、STEM像和SAED花样[19,35,47]
Fig.7 TEM images, STEM images, and selected area electron diffraction pattern of SLM NiTi alloys after heat treatment
(a-d) TEM images of SLM Ni50.4Ti49.6 after solution treatment (at 1000oC for 1 h) and ageing (at 350oC/450oC for 1 h)[47]
(e) STEM-HAADF image of SLM Ni51.4Ti48.6 after solution treatment (at 950oC for 12 h) and ageing (at 450oC for 5 h)[35]
(f-h) STEM-HAADF image and selected area electron diffraction pattern of SLM Ni51.1Ti48.9 after ageing (at 400oC for 1 h)[19]