选区激光熔化NiTi形状记忆合金研究进展
杨超, 卢海洲, 马宏伟, 蔡潍锶

Research and Development in NiTi Shape Memory Alloys Fabricated by Selective Laser Melting
YANG Chao, LU Haizhou, MA Hongwei, CAI Weisi
图4 SLM NiTi SMAs中形成缺陷的原因[19]以及能量密度对成形性的影响[22]
Fig.4 Defects in SLM NiTi SMAs (a-d)[19] and effect of energy density on formability of SLM NiTi SMAs (e-h)[22]