镁合金选区激光熔化增材制造技术研究现状与展望 |
彭立明, 邓庆琛, 吴玉娟, 付彭怀, 刘子翼, 武千业, 陈凯, 丁文江 |
Additive Manufacturing of Magnesium Alloys by Selective Laser Melting Technology: A Review |
PENG Liming, DENG Qingchen, WU Yujuan, FU Penghuai, LIU Ziyi, WU Qianye, CHEN Kai, DING Wenjiang |
图9 SLM态GZ151K方块中纵截面的裂纹分布[ |
Fig.9 Crack distribution in longitudinal section of the as-built GZ151K cube[ |
![]() |