原位激光定向能量沉积NiTi形状记忆合金的微观结构和力学性能
陈斐1,2,3(), 邱鹏程1, 刘洋1,2, 孙兵兵4, 赵海生4, 沈强1
Microstructure and Mechanical Properties of NiTi Shape Memory Alloys by In Situ Laser Directed Energy Deposition
CHEN Fei1,2,3(), QIU Pengcheng1, LIU Yang1,2, SUN Bingbing4, ZHAO Haisheng4, SHEN Qiang1

图7. 不同激光能量密度下NiTi合金的DSC曲线

Fig.7. DSC curves of as-built NiTi alloys with E = 20.0 J/mm2 (a), 21.7 J/mm2 (b), 23.3 J/mm2 (c), and 25.0 J/mm2 (d) (Ms—martensitic transformation start temperature, Mf—martensitic transformation end temperature, As—austenite transformation start temperature, Af—austenite transformation end temperature, ΔHM→A—austenite transformation enthalpy, ΔHA→M—martensite transformation enthalpy)