原位激光定向能量沉积NiTi形状记忆合金的微观结构和力学性能
|
|
Microstructure and Mechanical Properties of NiTi Shape Memory Alloys by In Situ Laser Directed Energy Deposition
|
|
图6. 不同激光能量密度下NiTi合金的TEM像和选区电子衍射花样 |
Fig.6. TEM images of as-built NiTi alloys with E = 20.0 J/mm2 (a), 21.7 J/mm2 (b), 23.3 J/mm2 (c), and 25.0 J/mm2 (d) (Inset in Fig.6a shows the corresponding SAED pattern) |
![]() |