原位自生2%TiB2 颗粒对2024Al增材制造合金组织和力学性能的影响 |
| 孙腾腾, 王洪泽, 吴一, 汪明亮, 王浩伟 |
|
Effect ofIn Situ 2%TiB2 Particles on Microstructure and Mechanical Properties of 2024Al Additive Manufacturing Alloy |
| SUN Tengteng, WANG Hongze, WU Yi, WANG Mingliang, WANG Haowei |
| 图10 热处理态2024Al合金及2024Al-2%TiB2合金应变硬化速率和真应力-真应变曲线 |
| Fig.10 True tensile stress-strain curves and work hardening rate (θ) of as-T6 2024Al and as-T6 2024Al-2%TiB2 alloys |
|