原位自生2%TiB2 颗粒对2024Al增材制造合金组织和力学性能的影响 |
| 孙腾腾, 王洪泽, 吴一, 汪明亮, 王浩伟 |
|
Effect ofIn Situ 2%TiB2 Particles on Microstructure and Mechanical Properties of 2024Al Additive Manufacturing Alloy |
| SUN Tengteng, WANG Hongze, WU Yi, WANG Mingliang, WANG Haowei |
| 图1 拉伸试样及微观组织观察试样取样示意图 |
| Fig.1 Schematic of tensile test specimen and the site of the microstructure characterization part (unit: mm) |
|