选区激光熔化 γ' 相强化镍基高温合金裂纹形成机理与抗裂纹设计研究进展
祝国梁, 孔德成, 周文哲, 贺戬, 董安平, 疏达, 孙宝德

Research Progress on the Crack Formation Mechanism and Cracking-Free Design of γ' Phase Strengthened Nickel-Based Superalloys Fabricated by Selective Laser Melting
ZHU Guoliang, KONG Decheng, ZHOU Wenzhe, HE Jian, DONG Anping, SHU Da, SUN Baode
图7 连续波和脉冲波模式下同一点(P2)的温度分布、冷却速率与时间的关系,以及连续波模式和脉冲波模型下制造的IN738LC合金的缺陷[57]
Fig.7 Calculated thermal history (temperature profiles, heating and cooling rates) versus time of the same point under the continuous-wave (a) and pulsed-wave modes (b), and the defect of the selective laser melted IN738LC alloys fabricated under the continuous-wave (c) and pulsed-wave mode (d)[57] (Tmax is the maximum temperature of the molten pool, dTdtmin is minimum cooling rate)