电弧熔丝增材制造2Cr13合金组织与性能各向异性行为 |
| 葛进国, 卢照, 何思亮, 孙妍, 殷硕 |
|
Anisotropy in Microstructures and Mechanical Properties of 2Cr13 Alloy Produced by Wire Arc Additive Manufacturing |
| GE Jinguo, LU Zhao, HE Siliang, SUN Yan, YIN Shuo |
| 图7 不同层间停留温度下垂直面铁素体相极图 |
| Fig.7 Pole figures of ferrite phase in the vertical plane for different interlayer dwelling temperatures (a) 550oC (b) 180oC (c) 150oC (d) 110oC |
|