电弧熔丝增材制造2Cr13合金组织与性能各向异性行为 |
| 葛进国, 卢照, 何思亮, 孙妍, 殷硕 |
|
Anisotropy in Microstructures and Mechanical Properties of 2Cr13 Alloy Produced by Wire Arc Additive Manufacturing |
| GE Jinguo, LU Zhao, HE Siliang, SUN Yan, YIN Shuo |
| 图1 电弧熔丝增材制造(WAAM) 2Cr13拉伸试样取样位置及其尺寸示意图 |
| Fig.1 Schematics of wire arc additive manufactured (WAAM) 2Cr13 part showing the positions of tensile samples (a) and its dimension (unit: mm) (b) |
|