粉末粒径对AlSi10Mg合金选区激光熔化成形的影响 |
| 王孟, 杨永强, Trofimov Vyacheslav, 宋长辉, 周瀚翔, 王迪 |
|
Effects of Particle Size on Processability of AlSi10Mg Alloy Manufactured by Selective Laser Melting |
| WANG Meng, YANG Yongqiang, Trofimov Vyacheslav, SONG Changhui, ZHOU Hanxiang, WANG Di |
| 图2 3种粒径AlSi10Mg粉末粒径分布及SEM像 |
| Fig.2 Particle size distribution (a) and SEM images of PSD1 (b), PSD2 (c), and PSD3 (d) (D10, D50, and D90 indicate 10%, 50%, and 90% cumulative particle sizes, respectively) |
|