激光摆动对激光熔化沉积钛合金微观组织及力学性能的影响 |
| 方远志, 戴国庆, 郭艳华, 孙中刚, 刘红兵, 袁秦峰 |
|
Effect of Laser Oscillation on the Microstructure and Mechanical Properties of Laser Melting Deposition Titanium Alloys |
| FANG Yuanzhi, DAI Guoqing, GUO Yanhua, SUN Zhonggang, LIU Hongbing, YUAN Qinfeng |
| 图4 不同激光摆动频率和摆动幅度下直线型激光摆动单道试样Nos.L1~L12的纵截面OM像 |
| Fig.4 Longitudinal section OM images of single-track samples Nos.L1-L12 (a-l) with linear laser oscillation under different frequencies and amplitudes |
|