激光热力交互增材制造Ti6Al4V合金的组织及力学性能 |
| 卢海飞, 吕继铭, 罗开玉, 鲁金忠 |
|
Microstructure and Mechanical Properties of Ti6Al4V Alloy by Laser Integrated Additive Manufacturing with Alternately Thermal/Mechanical Effects |
| LU Haifei, LV Jiming, LUO Kaiyu, LU Jinzhong |
| 图8 SLM和SLM-LSP拉伸试样的工程应力-应变曲线 |
| Fig.8 Engneering stress-strain curves of the tensile SLM and SLM-LSP specimens |
|