搅拌摩擦增材制造技术研究进展 |
| 李会朝, 王彩妹, 张华, 张建军, 何鹏, 邵明皓, 朱晓腾, 傅一钦 |
|
Research Progress of Friction Stir Additive Manufacturing Technology |
| LI Huizhao, WANG Caimei, ZHANG Hua, ZHANG Jianjun, HE Peng, SHAO Minghao, ZHU Xiaoteng, FU Yiqin |
| 图7 方形原料条增材装置原理图 |
| Fig.7 Schematics of an additive device for square raw material strips (a) 3D cross-sectional view of the additive device (b) plane cutaway view of the container of the system |
|