搅拌摩擦增材制造技术研究进展 |
| 李会朝, 王彩妹, 张华, 张建军, 何鹏, 邵明皓, 朱晓腾, 傅一钦 |
|
Research Progress of Friction Stir Additive Manufacturing Technology |
| LI Huizhao, WANG Caimei, ZHANG Hua, ZHANG Jianjun, HE Peng, SHAO Minghao, ZHU Xiaoteng, FU Yiqin |
| 图1 搅拌摩擦增材制造(FSAM)方法分类 |
| Fig.1 Classification of friction stir additive manufacturing (FSAM) methods |
|