金属激光增材制造材料设计研究进展 |
| 宋波, 张金良, 章媛洁, 胡凯, 方儒轩, 姜鑫, 张莘茹, 吴祖胜, 史玉升 |
|
Research Progress of Materials Design for Metal Laser Additive Manufacturing |
| SONG Bo, ZHANG Jinliang, ZHANG Yuanjie, HU Kai, FANG Ruxuan, JIANG Xin, ZHANG Xinru, WU Zusheng, SHI Yusheng |
| 图9 非晶合金的连续冷却转变曲线示意图及制备的铁基非晶合金结构[ |
| Fig.9 Schematic of continuous cooling transformation (CCT) curve of amorphous alloy (a) and Fe-based amorphous structure (b)[ |
|