金属激光增材制造材料设计研究进展 |
| 宋波, 张金良, 章媛洁, 胡凯, 方儒轩, 姜鑫, 张莘茹, 吴祖胜, 史玉升 |
|
Research Progress of Materials Design for Metal Laser Additive Manufacturing |
| SONG Bo, ZHANG Jinliang, ZHANG Yuanjie, HU Kai, FANG Ruxuan, JIANG Xin, ZHANG Xinru, WU Zusheng, SHI Yusheng |
| 图8 NbMoTaX合金的凝固路径和裂纹敏感性指数[ |
| Fig.8 Solidification path (a) and crack sensitivity index (b) of NbMoTaX alloy[ |
|