金属激光增材制造材料设计研究进展 |
| 宋波, 张金良, 章媛洁, 胡凯, 方儒轩, 姜鑫, 张莘茹, 吴祖胜, 史玉升 |
|
Research Progress of Materials Design for Metal Laser Additive Manufacturing |
| SONG Bo, ZHANG Jinliang, ZHANG Yuanjie, HU Kai, FANG Ruxuan, JIANG Xin, ZHANG Xinru, WU Zusheng, SHI Yusheng |
| 图6 SLM成形不锈钢和铁基非晶/不锈钢材料微观组织及腐蚀性能[ |
| Fig.6 Microstructures and corrosion properties of SLM-fabricated stainless steel and Fe-based amorphous/stainless steel (a, b) microstructures before (a) and after (b) polishing[ |
|