短程有序对高层错能Cu-Mn合金拉-拉疲劳变形行为及损伤机制的影响 |
| 韩冬, 张炎杰, 李小武 |
|
Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies |
| HAN Dong, ZHANG Yanjie, LI Xiaowu |
| 图14 应力幅90 MPa下Cu-Mn合金疲劳后裂纹源区形貌的SEM像 |
| Fig.14 SEM images showing the morphologies of fatigue source zone on the fracture surface of Cu-5%Mn (a), Cu-10%Mn (b), Cu-15%Mn (c), and Cu-20%Mn (d) alloys fatigued at a stress amplitude of 90 MPa |
|