短程有序对高层错能Cu-Mn合金拉-拉疲劳变形行为及损伤机制的影响 |
| 韩冬, 张炎杰, 李小武 |
|
Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies |
| HAN Dong, ZHANG Yanjie, LI Xiaowu |
| 图11 双对数坐标下S-N曲线示意图 |
| Fig.11 Schematic of S-N curves in a lg-lg scale showing the effect of σ |
|