短程有序对高层错能Cu-Mn合金拉-拉疲劳变形行为及损伤机制的影响 |
| 韩冬, 张炎杰, 李小武 |
|
Effect of Short-Range Ordering on the Tension-Tension Fatigue Deformation Behavior and Damage Mechanisms of Cu-Mn Alloys with High Stacking Fault Energies |
| HAN Dong, ZHANG Yanjie, LI Xiaowu |
| 图7 应力幅对Cu-20%Mn合金拉-拉疲劳损伤开裂行为的影响 |
| Fig.7 Effect of the stress amplitude on the fatigue damage and cracking behaviors in tension-tension fatigue of Cu-20%Mn alloy (GB refers to grain boundary, and SB represents slip band) (a) 90 MPa (b) 115 MPa (c) 160 MPa |
|