单一 MX 型析出相强化马氏体耐热钢力学性能及蠕变行为 |
| 李小琳, 刘林锡, 李雅婷, 杨佳伟, 邓想涛, 王海丰 |
|
Mechanical Properties and Creep Behavior of MX-Type Precipitates Strengthened Heat Resistant Martensite Steel |
| LI Xiaolin, LIU Linxi, LI Yating, YANG Jiawei, DENG Xiangtao, WANG Haifeng |
| 图7 经HR + N处理后Fe-0.03C-10Cr-0.2Zr-0.3V钢在700℃时效1000 h后析出相的HRTEM像、FFT谱及IFFT谱 |
| Fig.7 HRTEM image (a), and FFT (b) and IFFT (c) diagrams of precipitate formed in Fe-0.03C-10Cr-0.2Zr-0.3V steel aged at 700oC for 1000 h after HR + N treatment |
|