GH2909低膨胀高温合金热处理中的组织演变行为 |
| 李钊, 江河, 王涛, 付书红, 张勇 |
|
Microstructure Evolution of GH2909 Low Expansion Superalloy During Heat Treatment |
| LI Zhao, JIANG He, WANG Tao, FU Shuhong, ZHANG Yong |
| 图4 锻态GH2909合金中Laves相元素分布的EPMA结果 |
| Fig.4 EPMA results of element distribution of Laves phase in wrought GH2909 alloy (SEM—secondary electron morphology, BSE—back-scaterred electron image) |
|