GH2909低膨胀高温合金热处理中的组织演变行为 |
| 李钊, 江河, 王涛, 付书红, 张勇 |
|
Microstructure Evolution of GH2909 Low Expansion Superalloy During Heat Treatment |
| LI Zhao, JIANG He, WANG Tao, FU Shuhong, ZHANG Yong |
| 图3 锻态GH2909合金中Laves相的TEM像及选区电子衍射(SAED)花样 |
| Fig.3 TEM image and selected area electron diffraction (SAED) patterns of Laves phase in as-received GH2909 alloy (a, b) bright field TEM image of blocky Laves phase and related SAED pattern (c, d) bright field TEM image of short rod-like Laves phase and related SAED pattern |
|