快速凝固Ti-Al-Nb合金B2相形成机制与显微力学性能 |
| 梁琛, 王小娟, 王海鹏 |
|
Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy |
| LIANG Chen, WANG Xiaojuan, WANG Haipeng |
| 图1 落管无容器条件下Ti75 - x Al x Nb25合金的冷却速率及过冷度 |
| Fig.1 Calculated cooling rate (Rc) (a) and undercooling (ΔT) (b) of rapidly solidified Ti75 - x Al x Nb25 alloy via drop-tube technique (D—drop diameter) |
|