热处理温度对Ti0.5Zr1.5NbTa0.5Sn0.2 高熵合金组织结构与力学性能的影响
韩林至, 牟娟, 周永康, 朱正旺, 张海峰

Effect of Heat Treatment Temperature on Microstructure and Mechanical Properties of Ti0.5Zr1.5NbTa0.5Sn0.2 High-Entropy Alloy
HAN Linzhi, MU Juan, ZHOU Yongkang, ZHU Zhengwang, ZHANG Haifeng
图8 Ti0.5Zr1.5NbTa0.5Sn0.2高熵合金在2.5 × 103 s-1应变速率范围内的断口形貌
Fig.8 Fracture morphologies of Ti0.5Zr1.5NbTa0.5Sn0.2 HEA at 2.5 × 103 s-1 strain rate
(a) side macro morphology of fracture sample (b) as-cast
(c) 800oC, quenching (d) 1000oC, quenching
(e) 1200oC, quenching (f) 1400oC, quenching