热处理温度对Ti0.5Zr1.5NbTa0.5Sn0.2 高熵合金组织结构与力学性能的影响 |
| 韩林至, 牟娟, 周永康, 朱正旺, 张海峰 |
|
Effect of Heat Treatment Temperature on Microstructure and Mechanical Properties of Ti0.5Zr1.5NbTa0.5Sn0.2 High-Entropy Alloy |
| HAN Linzhi, MU Juan, ZHOU Yongkang, ZHU Zhengwang, ZHANG Haifeng |
| 图6 不同状态Ti0.5Zr1.5NbTa0.5Sn0.2高熵合金的准静态压缩侧面形貌 |
| Fig.6 Lateral morphologies of Ti0.5Zr1.5NbTa0.5Sn0.2 alloy with different states after quasi-static compression tests (a) as-cast (b) 800oC, quenching (c) 1000oC, quenching (d) 1200oC, quenching (e) 1400oC, quenching |
|