热处理温度对Ti0.5Zr1.5NbTa0.5Sn0.2 高熵合金组织结构与力学性能的影响 |
| 韩林至, 牟娟, 周永康, 朱正旺, 张海峰 |
|
Effect of Heat Treatment Temperature on Microstructure and Mechanical Properties of Ti0.5Zr1.5NbTa0.5Sn0.2 High-Entropy Alloy |
| HAN Linzhi, MU Juan, ZHOU Yongkang, ZHU Zhengwang, ZHANG Haifeng |
| 图5 Ti0.5Zr1.5NbTa0.5Sn0.2高熵合金准静态压缩性能 |
| Fig.5 Quasi-static compression properties of Ti0.5Zr1.5NbTa0.5Sn0.2 HEA (a) stress-strain curves at 5 × 10-4 s-1 strain rate (b) variation trend of yield strenghand microhardness with heat treatment temperature |
|