热处理温度对Ti0.5Zr1.5NbTa0.5Sn0.2 高熵合金组织结构与力学性能的影响
韩林至, 牟娟, 周永康, 朱正旺, 张海峰

Effect of Heat Treatment Temperature on Microstructure and Mechanical Properties of Ti0.5Zr1.5NbTa0.5Sn0.2 High-Entropy Alloy
HAN Linzhi, MU Juan, ZHOU Yongkang, ZHU Zhengwang, ZHANG Haifeng
图3 不同状态Ti0.5Zr1.5NbTa0.5Sn0.2高熵合金的微观形貌
Fig.3 BSE (a-e) and TEM (f) images of Ti0.5Zr1.5NbTa0.5Sn0.2 HEA with different states (Inset shows the SAED pattern)
(a) as-cast (b) 800oC, quenching (c) 1000oC, quenching (d) 1200oC, quenching (e, f) 1400oC, quenching