热处理温度对Ti0.5Zr1.5NbTa0.5Sn0.2 高熵合金组织结构与力学性能的影响 |
| 韩林至, 牟娟, 周永康, 朱正旺, 张海峰 |
|
Effect of Heat Treatment Temperature on Microstructure and Mechanical Properties of Ti0.5Zr1.5NbTa0.5Sn0.2 High-Entropy Alloy |
| HAN Linzhi, MU Juan, ZHOU Yongkang, ZHU Zhengwang, ZHANG Haifeng |
| 图2 不同状态Ti0.5Zr1.5NbTa0.5Sn0.2高熵合金的bcc相晶格常数 |
| Fig.2 Lattice constants of bcc phases in the Ti0.5Zr1.5NbTa0.5Sn0.2 HEA with different states |
|