SiCf/TiAl复合材料界面反应及热稳定性 |
| 沈莹莹, 张国兴, 贾清, 王玉敏, 崔玉友, 杨锐 |
|
Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites |
| SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui |
| 图6 SiCf/TiAl复合材料800℃界面反应层长大动力学曲线 |
| Fig.6 Interfacial reaction kinetic curves of SiCf/TiAl composites at 800oC (t—thermal exposure time) |
|