液氮温度下纯Ti动态塑性变形中的孪晶变体选择 |
| 高栋, 周宇, 于泽, 桑宝光 |
|
Selection of Twin Variants in Dynamic Plastic Deformation of Pure Ti at Liquid Nitrogen Temperature |
| GAO Dong, ZHOU Yu, YU Ze, SANG Baoguang |
| 图3 液氮温度下DPD后纯Ti中不同类型孪晶的微观结构 |
| Fig.3 Microstructures of typical areas in pure Ti after DPD at liquid nitrogen temperature (a) secondary twin (b, d) double twin (c) tertiary twin |
|