液氮温度下纯Ti动态塑性变形中的孪晶变体选择 |
| 高栋, 周宇, 于泽, 桑宝光 |
|
Selection of Twin Variants in Dynamic Plastic Deformation of Pure Ti at Liquid Nitrogen Temperature |
| GAO Dong, ZHOU Yu, YU Ze, SANG Baoguang |
| 图2 动态塑性变形(DPD)前后纯Ti的微观组织与孪晶分布 |
| Fig.2 EBSD images (a, b), (0001) pole figures (c, d), and image quality maps (e, f) of pure Ti before (a, c, e) and after (b, d, f) dynamic plastic deformation (DPD) |
|