液氮温度下纯Ti动态塑性变形中的孪晶变体选择
高栋, 周宇, 于泽, 桑宝光

Selection of Twin Variants in Dynamic Plastic Deformation of Pure Ti at Liquid Nitrogen Temperature
GAO Dong, ZHOU Yu, YU Ze, SANG Baoguang
图1 纯Ti样品取样示意图
Fig.1 Schematic of the seleced position of pure Ti sample (ND—normal direction, TD—transverse direction, RD—rolling direction)