喷射成形过共晶AlSiCuMg合金的固溶行为 |
| 冯迪, 朱田, 臧千昊, 李胤樹, 范曦, 张豪 |
|
Solution Behavior of Spray-Formed Hypereutectic AlSiCuMg Alloy |
| FENG Di, ZHU Tian, ZANG Qianhao, LEE Yunsoo, FAN Xi, ZHANG Hao |
| 图2 Al25Si4Cu1Mg合金的XRD谱 |
| Fig.2 XRD spectra of Al25Si4Cu1Mg alloy |
|