淬火速率对7136铝合金应力腐蚀开裂敏感性的影响 |
| 马志民, 邓运来, 刘佳, 刘胜胆, 刘洪雷 |
|
Effect of Quenching Rate on Stress Corrosion Cracking Susceptibility of 7136 Aluminum Alloy |
| MA Zhimin, DENG Yunlai, LIU Jia, LIU Shengdan, LIU Honglei |
| 图1 末端淬火示意图及慢应变速率拉伸试样尺寸 |
| Fig.1 Schematic of end quenching and drawing of slow strain rate tensile sample (unit: mm; ED—extruded direction, ND—normal direction, TD—transverse direction; blue indicates the part in the water, gray indicates the part in the air) |
|