选区激光熔化AlSi10Mg-Er-Zr合金微观组织及力学性能强化 |
| 杨天野, 崔丽, 贺定勇, 黄晖 |
|
Enhancement of Microstructure and Mechanical Property of AlSi10Mg-Er-Zr Alloys Fabricated by Selective Laser Melting |
| YANG Tianye, CUI Li, HE Dingyong, HUANG Hui |
| 图8 SLM成形AlSi10Mg-Er-Zr试样中合金元素分布 |
| Fig.8 Alloying element distributions of AlSi10Mg-Er-Zr sample fabricated by SLM (a) high angle annular dark field (HAADF) image of area scanning region (b) element distribution map (c) Al element (d) Si element (e) Mg element (f) Er element (g) Zr element |
|