选区激光熔化AlSi10Mg-Er-Zr合金微观组织及力学性能强化 |
| 杨天野, 崔丽, 贺定勇, 黄晖 |
|
Enhancement of Microstructure and Mechanical Property of AlSi10Mg-Er-Zr Alloys Fabricated by Selective Laser Melting |
| YANG Tianye, CUI Li, HE Dingyong, HUANG Hui |
| 图6 SLM成形AlSi10Mg-Er-Zr试样TEM像及HRTEM像 |
| Fig.6 TEM image and HRTEM images of AlSi10Mg-Er-Zr sample fabricated by SLM (a) TEM image of AlSi10Mg-Er-Zr sample (b) HRTEM image and fast fourier transform (inset) of Al3(Er, Zr) phase (c) HRTEM image and fast fourier transform (inset) of Mg2Si phase |
|